Santron
CHEMICAL, ELECTRICAL PROPERTIES AND
PROCESSING DATA OF SANTRON SAN RESIN

CHEMICAL PROPERTIES
Resistant to broad range of chemicals

ELECTRICAL PROPERTIES
Good Electrical Insulation property.

Dielectric strength KV/mm 30 (approx.)
Volume Resistivity Ohm-cm 1015(approx.)
Comparative Tracking Index   > 450

PROCESSING DATA
1) Injection moulding

a) Raw material pre-heating temp. = 85-105 deg c for the period of 3 hours ( based on various grades )
b) M/c cylinder temp. = 165 - 240 deg c ( based on various grades )

2) Extrusion

a) Extruder temp. = 215 - 230 deg c
b) Die temp = 210 - 220 deg c