| CHEMICAL,
ELECTRICAL PROPERTIES AND PROCESSING DATA OF SANTRON SAN
RESIN |
| CHEMICAL PROPERTIES: |
Resistant to broad range of
chemicals |
| ELECTRICAL PROPERTIES: |
Good Electrical Insulation
property. |
|
| Dielectric strength |
KV/mm |
30 (approx.) |
| Volume Resistivity |
Ohm-cm |
1015 (approx.) |
| Comparative Tracking Index |
>
450 |
> 450 |
|
|
PROCESSING DATA :
1) Injection moulding :
a) Raw material pre-heating temp. = 85-105 deg c for the period
of 3 hours ( based on various grades )
b) M/c cylinder temp. = 165 - 240 deg c ( based on various grades
)
2) Extrusion :
a) Extruder temp. = 215 - 230 deg c
b) Die temp = 210 - 220 deg c |
| |